///Steel parts rust after cutting
Cut quality & parts

Steel parts rust after cutting

Wet steel parts flash-rust quickly.

Safety first: Switch off the pump, release all pressure (open the on/off valve or bleed-down valve) and lock out before you open any high-pressure part. Never put a hand or tool near a running jet.
1Check the causes, most likely first 0 of 1 checked
01Parts stay wet Most likely

Water stays on the parts.

How to check: Dry parts and use a rust inhibitor in the tank.

PhotoArt. no.DescriptionReplaces OEMExcl. VAT
12145 Cable guide assy, L, C-5462-1
AssemblyFlow, H2O
Flow C-5462-1 € 357.00
12146 Cable guide assy, R, C-5461-1
AssemblyFlow, H2O
Flow C-5461-1 € 357.00
20290 PP honeycomb panels, 40mm, pure water only (2500 x 1220 mm)
Panel
— € 106.80
20291 PP honeycomb panels, 60mm, pure water only (2500 x 1220 mm)
Panel
— € 149.88
20292 PP honeycomb panels, 100 mm, Pure water and Abrasive (2500 x 1220 mm)
Panel
— € 358.80

Related problems

General advice based on manufacturer manuals and service practice. Always follow the manual of your machine. Not sure? .