Composite or laminate delaminates

Water pressure can lift layers at the pierce.

Safety first: Switch off the pump, release all pressure (open the on/off valve or bleed-down valve) and lock out before you open any high-pressure part. Never put a hand or tool near a running jet.
1Check the causes, most likely first 0 of 2 checked
01Pierce pressure too high Most likely

Stagnation pressure splits the layers.

How to check: Use low-pressure or drilled pierce.

PhotoArt. no.DescriptionReplaces OEMExcl. VAT
10640 Pressure switch, 60 PSI, 05142062
Gauge & sensorKMT
KMT 05142062 € 274.80
10641 Pressure switch, 30 PSI, 05140751
Gauge & sensorKMT
KMT 05140751 € 278.40
10691 Manometer 6000 PSI / 400 Bar
Gauge & sensorKMT, BFT, Flow, WSI
— € 76.80
10692 Manometer 80000 PSI / 5500 Bar
Gauge & sensorKMT, BFT, Flow, OMAX
— € 860.40
10782 Hyd. Pressure Gauge, 0-400 Bar, 05045497
Gauge & sensorKMT
KMT 05045497 € 114.00

02Abrasive interruption Possible

Pure water wedges the layers.

How to check: Ensure steady abrasive.